#General information ITEM section %ITEM SERIAL NUMBER 20220900208259 Mfr serial number STN12566-08259 #Test information Test section %TEST TEST DATE (DD/MM/YYYY) 23/02/2002 PROBLEM NO PASSED YES Run number 20220900208259 #Test data Data section %DATA TEMPERATURE (C) 28 I_LEAK150V (microA) 0.09754 I_LEAK350V (microA) 0.14579 Substr Origin 246 Substr Orient 111 Substr R Upper (kOhm.cm) 8 Substr R Lower (kOhm.cm) 4 Thickness (micron) 289 Vdep (V) 75 R Bias Upper (MOhm) 1.53 R Bias Lower (MOhm) 1.35 #Comment section %COMMENT #Defects section %DEFECT #DEFECT NAME Implant-Open Implant-Short Oxide-Punchthrough Pinhole Short Open %WEBLINK #DESCRIPTION URL #IV raw data Raw data section %RAWDATA DATA #IV 10 33.48 20 45.12 30 51.54 40 56.54 50 60.72 60 64.72 70 68.92 80 73.17 90 77.22 100 81.06 110 84.63 120 88.04 130 91.39 140 94.51 150 97.54 160 100.45 170 103.37 180 106.13 190 108.81 200 111.45 210 114.07 220 116.58 230 119.04 240 121.44 250 123.8 260 126.2 270 128.49 280 130.76 290 132.98 300 135.24 310 137.39 320 139.53 330 141.67 340 143.8 350 145.79 #CV 10 15 O.L. 20 O.L. 25 2887.7 30 2490.23 35 2212.33 40 2003.44 45 1844.22 50 1715.97 55 1612.7 60 1533.9 65 1480.41 70 1448.72 75 1432.26 80 1424.41 85 1420.56 90 1418.33 95 1416.62 100 1415.43 105 1414.45 110 1413.49 115 1412.75 120 1411.82 #End of manufacturer data file