#General information ITEM section %ITEM SERIAL NUMBER 20220900211290 Mfr serial number STN13241-11290 #Test information Test section %TEST TEST DATE (DD/MM/YYYY) 31/07/2002 PROBLEM NO PASSED YES Run number 20220900211290 #Test data Data section %DATA TEMPERATURE (C) 26 I_LEAK150V (microA) 0.13517 I_LEAK350V (microA) 0.209 Substr Origin 293 Substr Orient 111 Substr R Upper (kOhm.cm) 8 Substr R Lower (kOhm.cm) 4 Thickness (micron) 291 Vdep (V) 75 R Bias Upper (MOhm) 1.52 R Bias Lower (MOhm) 1.33 #Comment section %COMMENT #Defects section %DEFECT #DEFECT NAME Implant-Open Implant-Short Oxide-Punchthrough Pinhole Short Open %WEBLINK #DESCRIPTION URL #IV raw data Raw data section %RAWDATA DATA #IV 10 41.31 20 58.07 30 67.65 40 75.23 50 81.75 60 87.77 70 93.62 80 99.54 90 105.38 100 110.99 110 116.28 120 121.32 130 126.14 140 130.8 150 135.17 160 139.71 170 143.88 180 148.06 190 152.14 200 156.14 210 160.08 220 163.93 230 167.73 240 171.46 250 175.1 260 178.7 270 182.3 280 185.8 290 189.2 300 192.6 310 195.9 320 199.4 330 202.6 340 205.8 350 209 #CV 10 15 O.L. 20 O.L. 25 2965.79 30 2554.41 35 2268.68 40 2052.41 45 1885.69 50 1753.83 55 1646.41 60 1563.04 65 1502.02 70 1461.77 75 1438.22 80 1425.75 85 1419.48 90 1416.16 95 1414.05 100 1412.54 105 1411.37 110 1409.87 115 1409.04 120 1408.13 #End of manufacturer data file